| dc.rights.license | http://creativecommons.org/licenses/by-nc-sa/3.0/ve/ | |
| dc.contributor.author | Meléndez, Hildemaro | |
| dc.contributor.author | Rondón, Jairo | |
| dc.contributor.author | Cabrera, Marbelia | |
| dc.contributor.author | García, Edder | |
| dc.contributor.author | Lugo, Claudio | |
| dc.contributor.author | Quintero, Mahiceth | |
| dc.contributor.author | Pérez, Manuel | |
| dc.contributor.author | Del Castillo Paredes, Hector Luis | |
| dc.date.accessioned | 2010-05-19T20:48:40Z | |
| dc.date.available | 2010-05-19T20:48:40Z | |
| dc.date.issued | 2010-05-19T20:48:40Z | |
| dc.identifier.issn | 1856-3201 | es_VE |
| dc.identifier.uri | http://www.saber.ula.ve/handle/123456789/31062 | |
| dc.description.abstract | La conversión de n-pentano y su selectividad hacia la isomerización son afectadas por cambios en la acidez del catalizador. Para este estudio se utilizó como soporte el sólido mesoporoso MCM-41, al cual se le incorporó Pt por el método de intercambio iónico en estado sólido, y el ácido tungstenofosfórico (H3[P(W3O10)4]× H2O (HPW)) en solución alcohólica. Las pruebas catalíticas se llevaron a cabo a 350ºC en flujo de hidrógeno. El catalizador se caracterizó mediante las siguientes técnicas: DRX, Adsorción de N2, MET, TPD-NH3 y Difracción de electrones. La mayor actividad se obtuvo cuando se utilizó el
catalizador 30%HPW/70%(1%Pt/MCM-41). | es_VE |
| dc.language.iso | es | es_VE |
| dc.rights | info:eu-repo/semantics/openAccess | |
| dc.subject | Isomerización | es_VE |
| dc.subject | N-pentano | es_VE |
| dc.subject | Mesoporosos | es_VE |
| dc.subject | Ácido tungsteno fosfórico y platino | es_VE |
| dc.title | Efecto del tiempo de inmersión de superficies de SiO2 en silano sobre la deter-minación de un mojado intermedio mediante la medición de ángulos de contacto | es_VE |
| dc.type | info:eu-repo/semantics/article | |
| dc.description.abstract1 | Conversion of n-pentane and selectivity to isomerisation are affected by changes in the acidity of the catalyst. In this study, the mesoporous MCM-41was used as the support, and Pt was incorporated by the method of solid-state ion exchange, and tungsten phosphoric acid (H3 [P (W3O10) 4] × H2O (HPW)) in alcohol solution. The catalytic tests were carried out at 350 °C in hydrogen flow. The catalyst was characterized by the following techniques: XRD, N2 adsorption, TEM, TPD-NH3 and electron diffraction. The 30% HPW/70% (1%Pt/MCM-41) was the most active. | es_VE |
| dc.description.colacion | 73-78 | es_VE |
| dc.description.frecuencia | cuatrimestre | es_VE |
| dc.identifier.depositolegal | 200502ME2052 | es_VE |
| dc.subject.departamento | Departamento de Química | es_VE |
| dc.subject.facultad | Facultad de Ciencias | es_VE |
| dc.subject.keywords | Isomerization | es_VE |
| dc.subject.keywords | N-pentane | es_VE |
| dc.subject.keywords | Mesoporous | es_VE |
| dc.subject.keywords | Tungsten phosphoric acid and platinum | es_VE |
| dc.subject.publicacionelectronica | Revista Avances en Química | es_VE |
| dc.subject.seccion | Revista Avances en Química: Notas Técnicas | es_VE |
| dc.subject.thematiccategory | Química | es_VE |
| dc.subject.tipo | Revistas | es_VE |
| dc.type.media | Texto | es_VE |